===704.3.2 Procedure===
 
===704.3.2 Procedure===
Concrete cylinders shall be tested for compressive strength according to AASHTO T 22. Test results and calculations shall be recorded through SiteManager.
+
Concrete cylinders shall be tested for compressive strength according to AASHTO T 22. Test results and calculations shall be recorded through AASHTOWARE Project (AWP).
  
 
===704.3.3 Sample Record===
 
===704.3.3 Sample Record===
The sample record shall be completed in SiteManager, as described in [[:Category:101 Standard Forms#Sample Record General Information| Sample Record General Information]] [[image:bulldozer.jpg|20px]]. Appropriate remarks, as described in [[106.20 Reporting|EPG 106.20 Reporting]], are to be included in the remarks to clarify conditions of acceptance or rejection. Test results shall be reported on the appropriate templates under the Tests tab.
+
The sample record shall be completed in SiteManager, as described in [[:Category:101 Standard Forms#Sample Record, General|AWP MA Sample Record, General]]. Appropriate remarks, as described in [[106.20 Reporting|EPG 106.20 Reporting]], are to be included in the remarks to clarify conditions of acceptance or rejection. Test results shall be reported on the appropriate templates under the Tests tab.

Revision as of 08:22, 14 September 2021

Approved Products
Qualified Rapid Set Concrete Patching Material (Horizontal)
Qualified Rapid Set Concrete Patching Material (Vertical and Overhead)

704.1 Construction Inspection for Sec 704

This work consists of removing deteriorated concrete, preparing the repair site, forming where required, placing and finishing new concrete or qualified special mortar and applying epoxy in the required areas.

The types of repair are:

  • Half-Sole Repair
  • Deck Repair With Void Tube Replacement
704.1 half sole.jpg
704.1 exposed.jpg
If the contractor can adequately patch an exposed void tube, then the entire repair is considered either half-sole or monolithic deck repair.
  • Full Depth Repair
  • Modified Deck Repair
  • Superstructure Repair (Unformed)
  • Slab Edge Repair
  • Substructure Repair (Formed)
  • Substructure Repair (Unformed)
  • Epoxy Sealing
  • Monolithic Deck Repair
  • Shallow Deck Repair

Refer to Sec 704.

Excavator hydraulic hammers shall not be used for removal of deck concrete unless otherwise specified on the bridge plans.

704.2 Materials Inspection for Sec 704

For more information regarding Rapid Set Concrete Patching Material, refer to JSP 02-01.

Two lists of qualified rapid set concrete patching materials are maintained by Construction Materials. One list shows approved horizontal patching materials and the other list is for vertical and overhead patching materials.

704.3 Laboratory Testing for Sec 704

704.3.1 Scope

This guidance establishes procedures for Laboratory testing and reporting concrete cylinders representing Class X Concrete.

704.3.2 Procedure

Concrete cylinders shall be tested for compressive strength according to AASHTO T 22. Test results and calculations shall be recorded through AASHTOWARE Project (AWP).

704.3.3 Sample Record

The sample record shall be completed in SiteManager, as described in AWP MA Sample Record, General. Appropriate remarks, as described in EPG 106.20 Reporting, are to be included in the remarks to clarify conditions of acceptance or rejection. Test results shall be reported on the appropriate templates under the Tests tab.

This category currently contains no pages or media.